Advanced Search

Journal Navigation

Journal Home

Subscriptions

Archive

Contact Us

Table of Contents

Sign In to gain access to subscriptions and/or personal tools.
Textile Research Journal
This Article
Right arrow Full Text (PDF)
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Email this article to a friend
Right arrow Similar articles in this journal
Right arrow Alert me to new issues of the journal
Right arrow Add to Saved Citations
Right arrow Download to citation manager
Right arrowRequest Permissions
Right arrow Request Reprints
Right arrow Add to My Marked Citations
Citing Articles
Right arrow Citing Articles via Google Scholar
Right arrow Citing Articles via Scopus
Google Scholar
Right arrow Articles by Weigmann, H.-D.
Right arrow Articles by Dansizer, C.
Right arrow Search for Related Content
Social Bookmarking
 Add to CiteULike   Add to Complore   Add to Connotea   Add to Del.icio.us   Add to Digg   Add to Reddit   Add to Technorati   Add to Twitter  
What's this?

Kinetics and Temperature Dependence of the Chemical Stress Relaxation of Wool Fibers

Hans-Dietrich Weigmann

Textile Reseurch Institute, Princetion, New Jersey

Ludwig Rebenfield

Textile Reseurch Institute, Princeton, New Jersey

Cornelia Dansizer

Textile Reseurch Institute, Princeton, New Jersey

The stress relaxation process of keratin fibers may be divided into two stages, the first rapid stage involving hydrogen bond breakdown and the second slower stage being connected with disulfide bond scission. The temperature dependence of the second disulfide-controlled stage of stress relaxation of wool fibers from extensions of 20 and 40% was investigated at pH 7.0, both in the presence and absence of the sulfhydryl- blocking agent N-ethylmalimide (NEMI). By plotting the relaxation modulus Er as a function of temperature, a transition at 70°C was observed for untreated wool fibers. An increase in the SH content by partial reduction of the wool cystine decreases this transition temperature, as was expected from previous evidence of the SH dependence of the transition temperature under stress obtained from stress-strain curves [20]. By normalizing the stress at any time with a stress value in the presence of the SH-group blocking agent, it was possible to eliminate the first stage of stress relaxation without losing any component of the second stage. The viscoelastic behavior of the second stage was found to approximate that of a single Maxwellian element. The controlling mechanism in 'this stage appears to be a disulfide interchange catalyzed by free. SH groups, with an activation energy of approximately 23 kcal mole, which is independent of the strain level.

Textile Research Journal, Vol. 36, No. 6, 535-542 (1966)