Advanced Search

Journal Navigation

Journal Home

Subscriptions

Archive

Contact Us

Table of Contents

Click here to sign up for SAGE Journal Email Alerts today!

Sign In to gain access to subscriptions and/or personal tools.
Textile Research Journal
This Article
Right arrow Full Text (PDF)
Right arrow References
Right arrow Alert me when this article is cited
Right arrow Alert me if a correction is posted
Services
Right arrow Email this article to a friend
Right arrow Similar articles in this journal
Right arrow Alert me to new issues of the journal
Right arrow Add to Saved Citations
Right arrow Download to citation manager
Right arrowRequest Permissions
Right arrow Request Reprints
Right arrow Add to My Marked Citations
Citing Articles
Right arrow Citing Articles via Google Scholar
Right arrow Citing Articles via Scopus
Google Scholar
Right arrow Articles by Pandey, S.N.
Right arrow Articles by Nair, P.
Right arrow Search for Related Content
Social Bookmarking
 Add to CiteULike   Add to Complore   Add to Connotea   Add to Del.icio.us   Add to Digg   Add to Reddit   Add to Technorati   Add to Twitter  
What's this?

Mercerized and Crosslinked Cotton Yarns

Part II: Effect of Stretching During Mercerization on Physical Properties and Degradation of Crosslinked Yarns

S.N. Pandey

Cotton Technological Research Laboratory, Matunga, Bombay 400 019, India

P. Nair

Cotton Technological Research Laboratory, Matunga, Bombay 400 019, India

The effect of varying degrees of stretch on various cotton yarn properties during mercerization was studied. Scoured cotton yarns were slack mercerized in an aqueous solution of caustic soda, then restretched to 90%, 94%, 96%, 100%, and 103% of the original lengths. There was a considerable increase in strength and a decrease in elon gation. Mercerized and scoured yams were subjected to a crosslinking treatment with formaldehyde using the Form W and D processes. The mercerized yarns had a higher formaldehyde content but retained higher strength compared to scoured crosslinked yarn for both crosslinking processes. The mercerized yarn samples stretched to 103% showed the highest strength retention values after crosslinking for both the processes compared to other yams. The scoured yams crosslinked by the Form D bath process showed very low tenacity retention (42%), while the yam mercerized and stretched to 103% showed very high tenacity retention (90%). The relationships between strength and various other properties are also discussed. The higher retention of tenacity in mercerized crosslinked yam is attributed to the removal of weak points present in cotton and the more uniform structure capable of distributing stress along the fibers.

Textile Research Journal, Vol. 57, No. 9, 532-538 (1987)